1、Low Cure Applications in PowderCoatingsWith Emphasis on FormulationSeptember 2024,Derick A Forcha,End-use SpecialistAgendaSeptember 2024Page 2Trends,Opportunities&ChallengesFormulation StrategyCatalyst SelectionAdditive Selection/DSC AnalysisKey TakeawaysDerick Forcha-Low Cure Applications in Powder

2、 CoatingsTrendsSeptember 2024 Derick Forcha-Low Cure Applications in Powder CoatingsPage 3Photo Credit:BYK-USA In our view the market for low cure applications in powdercoatings,will continue grow.OpportunitiesPage 4Acid/HydroxylResinAcid polyestersCrosslinkerHAA-OH FunctionalPolyestersCrosslinkersB

3、lockedisocyanatesUretidonesCatalyst-YesAcid/EpoxyResinsAcid PolyesterGMA acrylicCrosslinkersEpoxy resin/TGICCatalysts-YesEpoxyResinsCrosslinkersDICYPhenolicCatalyst-YesQuaternaryAmmonium saltsUnsaturatedSystemsIncrease opportunity for low cure Systems150C 220C140C 200C120C 210C115C 150CSource:(Modif

4、ied)Merfeld,G.et al.120C Cure,Durable,corrosion protection for temperature sensitive substrates,01/28/2005 https:/apps.dtic.milSeptember 2024 Derick Forcha-Low Cure Applications in Powder CoatingsChallenges of Low Cure Powder CoatingsSeptember 2024Derick Forcha-Low Cure Applications in Powder Coatin

5、gsPage 5120 C130 C135 C140 CVery difficult toProcess and StoreEasier to process and store,difficult to use on temp.sensitive substrateOptimal and Most appropriate temperaturewindow with current resin technologiesBetter BalanceEasy of good quality productExceptionPeroxide Cure ether UrethaneFormulati

6、on StrategyFormulation StrategySeptember 2024Page 7Starting point formulationStandard additives withDifferent melt pointsNo CatalystCure Window has shifted150C for 30 minsto 136C for 8 minsFormulators introducesCatalyst to reduce cureTime&TemperatureFormulator goes back to theFormula and choose addi

word格式文档无特别注明外均可编辑修改,预览文件经过压缩,下载原文更清晰!
三个皮匠报告文库所有资源均是客户上传分享,仅供网友学习交流,未经上传用户书面授权,请勿作商用。
本文主要探讨了粉末涂料中低固化应用的趋势、机遇与挑战,重点介绍了配方的策略,包括催化剂和添加剂的选择,并讨论了DSC分析在低固化粉末涂料配方中的应用。文中提到,低固化应用的市场将持续增长,机遇主要在于酸/羟基树脂、酸聚酯、交联剂等材料的应用。挑战包括在当前树脂技术下,寻找最优的固化温度窗口,以及加工和存储的难度。通过DSC分析,可以确定粉末的玻璃化转变温度和催化剂的影响,从而帮助配方师调整配方,优化固化过程。此外,还讨论了如何通过调整添加剂和分子质量来改善流平和表面质量。最后,文中强调了在低固化粉末涂料配方中,起始点配方、标准添加剂、催化剂选择和基于熔点行为及机制的添加剂包的重要性。
"低固化温度粉末涂料的最新趋势是什么?" "如何选择合适的催化剂以降低粉末涂料的固化时间?" "在低固化温度粉末涂料配方中,如何有效解决气泡和孔洞问题?"